32147-205 PMC3-27.5g

$ 760.00

 Product info:  產品資訊:
When fired at 900°C for two hours, PMC3™ is the strongest fine silver metal clay available. It has a finer, smoother composition that’s easy to work with and manipulate. You can also embed findings with confidence–firing at a low temperature means they won’t be heat-damaged. PMC3 is suitable for torch-firing as well as kiln-firing.
Composition: Metal powder (90%), water and organic binder (10%)
Shrinkage: 12%
Color: Pickle white
Physical Properties:
Firing temp.: 900°C for two hours to achieve highest hardness and maximum durability; or 600°C for 45 minutes; or 650°C for 20 minutes; or 700°C for 10 minutes.
Melting point: 960°C
Density after firing: 9.3 specific gravity (rolled silver = 10.5 specific gravity)
當在900℃下燒製兩小時後,PMC3™便成最強的純銀金屬銀粘土。它擁有更精細、更光滑的結構,易於使用和操作。另外它還有一強項 – 黏土可在較低溫度燒製,這意味著他們不易因過熱而損耗。 PMC3適合火炬點火以及窯燒製。
組合物:金屬粉末(90%),水和有機粘合劑(10%)
收縮率:12%
顏色:白
物理性質:
燒成溫度:900℃保溫2小時,以達到最高的硬度和最大的耐用性;或600℃45分鐘;或650℃,20分鐘;或700℃下進行10分鐘。
•熔點:960℃,
燒成後密度:9.3比重(軋銀=10.5比重)
Category:

Description

PMC3    27.8g

This Marvelous new Precious Metal Clay is a perfect way to finish your fused glass project. Firing as low as 600 degrees Celsius , fire it in your kiln or the new Hot Pot. It is now possible to add Fine Silver to tack fired pieces to add yet another dimension to your glass creations.

Product Description 產品說明:

Size: 25g
Brand: PMC3
Form: Clay
Country of origin: Japan

Shrinkage: ~12%

Methods:

1.Before you put your clay into a kiln, please make the clay dry with 180 ℃.
 2. Put your clay into the Kiln. Set the kiln to 800℃. when the kiln reaches the desired temperature, wait for 10 mins.
3. Turn the kiln off. After it is cooled down, take out the artwork.
尺寸:25克
品牌:PMC3
形態: 粘土
原產地:日本

收縮率: 約12%

燒製方法:

1.將作品放進窯前,請先用180℃把它烘乾。
2. 將作品放進窯,窒調至800℃,待窯的溫度上升至800℃後,等待約10分鐘。
3.將窯關閉,待窯降溫後,把作品取出。

 

 